Product DescriptionThe product owns excellent mechanical property
and the faster crosslink speed. Comply with Rohs and Reach,
applicable for building wire.Trade Mark and
Appilcation Trade MarkProduct
NameApplicationYT-1251E105ºC Silane-crosslinked halogen-free
low-smoke flame-retardant polyolefin cable materialApplicable for
pressure-extrusion and tube-extrusion, general performance flame
retardantPerformance IndexesNOTest
Items UnitYT-1251E1Appearance -Compliance2Density g/cm31.523Original
Tensile Strength Mpa12.54Original Elongation at
Break %1905Thermal AgeingTest Condition-158ºCx168hRentention
Rate of Tensile Strength%+15Retention Rate of Elongation at
Break%-156Low-temperature ImpactTest Conditions--40ºCFailure
(≤15/30)Piece07Oxygen Index %348Volume Resistivity
(20ºC) Ω.m1x10(12)9Dielectric Strength
(20ºC) MV/m2510Thermal ElongationTest Conditions-200 ºC 0.2Mpa
15minElongation Rate Under the load%30Permanent Change Rate after
cooling%011PH Value -612Conductivity μs/mm613Smoke
DensityWith FlameDs Max90Without FlameDs Max165Can be customized
according to customer's requirements. Use Methods1. Mixing: Mix the
component A and component B evenly, add them into the hopper. If
the color required, use the EVA base materials (the color
masterbatch should be dried). The material should be use up within
2 hours after unpacking. (It can't be dried). The external water
can' be brought in during the process. 2. Suggest to use equal
distance & unequal depth, single thread screw. 3. Extrusion
Temperature: Zone 1Zone 2Zone 3Zone
4NeckHead100±10125±10135±10140±10140±10140±104. Double color cable:
Color line can use component A and EVA base materials together,
without or with a small numner of component B. 5. Pay-off speed:
Without affecting of surface smoothness and perfirmance the faster,
the better. 6. Crosslink: Natural crosslink or water bath (Steam).
Natural Crosslink: Temperature 15-25ºC, crosslink will be finished
around 7 days. hen temperature is higher than 25ºC, crosslink will
be finished around 3 days. Water bath or Steam: should control the
temperature arond 60-70 ºC in order to keep it from sticking
together, it will finish about 4 hours. The thickness of the test
piece is 1mm. It thickness >1mm, the crosslink time should be
adjusted according to the actual situation. Full performance test,
water bath (steam) 65ºC, more than 8 hours, to ensure the material
is fully crosslinked. Package, Transport and Storage1. Package:
Vacuum packed. 2. Transport: Can't be exposed to the sun or rain,
or suffer mechanical damange. 3. Storage: Should be stacked on the
backing plate in a clean and dry warehouse. Valid Period: 12
months. /* January 22, 2024 19:08:37 */!function(){function
s(e,r){var
a,o={};try{e&&e.split(",").forEach(function(e,t){e&&(a=e.match(/(.*?):(.*)$/))&&1
Related products about 125 º C Cable Material for Pressure-Extrusion
- Waste Tyre Plastic Recycling Machinery Machine Tire Crusher Production Line Rubber Crumb Grinding Machine Equipment Tire Shredder
- Stretch Plastic Blowing Pet Bottle Making Blow Molding Machine Bottles Stretch Automatic Pet Bottle Blowing Machine
- Waste Plastic Pet Bottle, Water Bottle Flake, PP/HDPE/LDPE PE Film Jumbo Woven Bags Plastic Crusher Machine, Plastic Crushing Washing Recycling Machine
- Type 2 Wall-Mounted Electric Car Charging Station 7kw /11 Kwelectric Vehicle Charging Station Home Wallbox AC EV Charger Single Phase or 3three Phase
- G-View G12W Wholesale Auto Car LED Headlight Bulb High Power H13 H11 9005 H7 H4 Car LED Headlights LED Car Lights
- New Design Porcelain Round Plates Dinner Set for Wedding and Banquet
- China 2023 New Design Super Soft 100% Polyester Microfiber Knitted Oversized Decoration Hoodie Blanket
- Handmade Art Creative Materials Thickened White Paper Cup DIY Disposable Handmade Colored Paper Cup